Liebe Besucherinnen und Besucher,
aufgrund unseres Sommerfestes sind wir am 03. September 2026 bis 14 Uhr erreichbar. Am 04. September 2026 sind wir wieder wie gewohnt für Sie da. Vielen Dank für Ihr Verständnis.
Ihr Team von Sack Fachmedien
Buch, Englisch, 2020 Seiten, Format (B × H): 170 mm x 240 mm, Gewicht: 3700 g
ISBN: 978-0-87849-200-8
Verlag: Trans Tech Publications
This two-volume set contains a collection of 381 peer-reviewed papers. Its aim is to bring together the latest advances in, and applications of, alloy design, process development, component engineering, phase-composition prediction, high-temperature oxidation, wrought alloys, lifetime estimation and materials behavior, cobalt-based alloys, nickel-iron alloys, joining, alternative materials and powder-metallurgy and also to consider the future of superalloys.
Autoren/Hrsg.
Fachgebiete
Weitere Infos & Material
Sponsors, Committees and Preface
Test Analysis on Crack Propagation Rate of Axle Pipe Steel
Nanostructure formed by phase separation of fcc-Al from eutectic crystallization in the Al85Ni10Ce5 metallic glass
In Situ Test Study on Shear Strength Properties of Weathered Silty Mudstone
On the Tensile Experiments of the Woven Membrane Materials under Bi-Axial Loads
Behaviors of Carbon in Different Concentration of Sulfuric Acid
Fabrication of Thermo-Conductivity Film Using Anodic Aluminum Oxide Template and Silver Nanowires
Microstructure Evolution of a Metastable CrMnN Austenitic Stainless Steel during Compression Deformation
Study on the Formability of Different Gauge Tailor Welded Blanks Based on Tensile Test
Modified PP Fibers Reinforced Cement Mortar
Ex-Situ Study of Polymeric Syntactic Foams Mechanical Response Under Compression Loading: Effects of Foam Microstructure Using Microtomography Techniques
New Method for Measuring the Viscosity of the Molten Amorphous Alloy
Fundamental Aspects of Stray Current Corrosion on Buried Pipeline
Crystallographic Texture in SrM Hexaferrite Doped with Zn2+ Ions
Effect of the Mixing-Melt and Superheating on the Primary Si Phase of Hypereutectic Al-20%Si Alloy
The Effect of (Li,Ce) Doping in Aurivillius Phase Material Na0. 5Bi4.5Ti4O15
Lotus Fiber Production and its Property
Measuring Residual Stress of 304 Austenitic Stainless Steel by Spherical Indentation
Equal Channel Angular Pressing and Torsion (ECAPT) for Densification and Strengthening Properties of Powder Sintered Materials
Research on Casting of GH3030 Superalloy with Electromagnetic Stirring
Study on Desulfurizing Capability of XuanHua Steelworks Titanium Slag
Effect of Solute Depleted Area on the Distribution of MnS in Fe-3%Si
The Optimization of Aluminum Foam Compound Board Structure Based on Machine Acoustic Enclosure
Drop Impact Behavior of Packaging System with Irregular Honeycomb Core
Hydrogen Embrittlement and Corrosion Fatigue Performance of Galvanized Steel Wires for High Strength Bridge Cables
Rapid Fabrication of Micro Optical Elements Using DMD-Based Maskless Lithography Technique
Sr1-xNdXFe12O19 Ferrite Synthesized through Sol-Gel Self-Combustion
A New Method to Measure Inertial Parameters of Rigid Body Based on Energy Decay Theory
Aging Behavior of T91/10CrMo910 Dissimilar Steel Welded Joints
Influence of Low Tempering Temperature on Fracture Toughness of Ultra High Strength Boron Steel for Hot Forming
New Strength Criterion Based on Relationship between Elastic and Plastic Strains
Evolution of Recrystallization Microtexture of Cold-Rolling Low Carbon Sheet Steel Based on CSP during Batch Annealing
Effect of Microcracks on the Toughness of Particulate Composites
Fatigue Crack Propagation at Negative Stress Ratio in 2A12 Aluminum Alloy
Precipitation and Recrystallization Behaviors of a High-Nitrogen Austenitic Stainless Steel Aging at 90°C
Core Courses for Undergraduate Students in Materials Science and Engineering
Non-Local Stress and Stain Analysis at Crack Tip Based on Different Types of Weighted Functions
Relation between Medium-Range Order and Crystallization in Al-Ni Based Glass-Former Alloys
Comparison of Two Different Chemical Conversion Coating on Aluminum Alloy
Study on Property of Ti-Based Nonevoparobal Getter
Research on Design and Pavement Performance of TLA Modified Asphalt Mixture
The Mechanical Properties of PSA Fibers after Corrosion
Deformation Mechanism in the Mg-Gd-Y Alloys Predicted by Deformation Mechanism Maps
Research of Micromechanism on Residual Stress in Aluminum Alloy Thick Plate
Research on Cryogenic Properties of Different Fiber Asphalts and Mixtures
Tribological Performances and Friction Reduction Mechanism of N-Al2O3/FeS Solid Lubrication Duplex Layer
Microstructure Characterization of Large Strain Deformed Fe-32%Ni Alloy
Prediction of Fretting Fatigue Life of Aluminum Alloy LY12CZ
The Fuzzy Judgment for the Wearing Life Distrituion of the Rolling Bearing
Effect of Thermohydrogen Treatment Temperature on Machinability of Ti6Al4V Alloy
Effects of Sm on Microstructure and Mechanical Properties of Mg-5.5Al -0.5Y Alloy
Numerical Simulation of Flow Field in Bloom Continuous Casting Mold with Electromagnetic Stirring
Investigations on the Textured Bi3NbTiO9 Ceramics via Spark Plasma Sintering
Research on Internal Stress in Electroplated Cu Films on Fe Substrates and Ni Substrates - Based on Electron Theory
Effects of Cerium on the Microstructures and Electrochemical Properties of Al-Zn-Sn Sacrificial Anodes
Ageing Behaviour of a Cu-Cr-Zr Alloy under an Imposed Electric Current
The Electromagnetic Mechanism of Pulsed Electric Discharge on Directionally Solidified Microstructure of Pure Aluminum
Analysis of Carbide Precipitates in API X80 Medium-Thickness Plate
High Anticorrosive Properties of Hot-Dip 55 wt% Al-Zn-Si Coatings on Q235 Steel
Mechanical Properties of UPR Composite Synergistically Toughened by Rigid Nano-Particles
Effect of Thermal Relaxation on Propagation of Longitudinal Displacement Wave
Research on Damping of Foamed Al Composite Filled Epoxy Resin in the Holes
Elongational Rheology of LLDPE by Melt Spinning Technique
The Influence of Complexing Agent to the Function of Electroless Plating of P-Ni Alloy on Magnesium Alloy
Drag Reduction Effect of Dimples Arranged in Two-Dimensional Quasicrystal Structure
A Study on Morphologies of Second Phases in the Mg-Sr and Mg-Sr-Y Alloys
Effect of Asynchronous Rolling on Wear-Resisting Performance of High Manganese Steel
Performance Properties of Polymer Modified Cement Grouts for Repair and Rehabilitation of Concrete Pavement
Process of Equiaxed Grains of RE-Al Alloy under Slope Vibration
Fabrication of Maxillofacial Implant Using CAD CAM System
Mass Diffusivities of Radiata Pine in Superheated Steam Drying
Measurement of Surface Roughness by Computer Vision in Planning Operations
Micromechanical Strength of Particle in Composite Ceramic with Partial Debonding Interphase
Study on Bubble's Stability in Process of Preparing Foam Aluminum by Powder Metallurgy Method
Effect of the Interlamellar Spacing on Mechanical Properties of SWRS82B Wire Rod before and after Drawing
Manufacturing Basalt/Ramie Fibers Hybrid Reinforced PP Thermoplastic Panel
Effect of Ageing Process on Mechanical Properties of Martensite Precipitation-Hardening Stainless Steel
An Analytical Model of Wool Crimp
Probabilistic Integrity Assessment of Pressure Piping Containing Defects
Research on Flaw Detection for 3-D Braided Composite Material Using Ultrasonic Testing Based on Wavelet Packet Transform
Impact Behaviors of Flax/Polypropylene Weft Knitted Composites
Material Fatigue Behavior and its Mechanism Based on MMM Technology
Survey of Materials Testing Using Ultrasonic
Prospect Analysis on New Ironmaking Technology of Oxygen Blast Furnace and Gas-Recycle
Experimental Study on the Effect of Normal Stress on the Shear Banding in a Zr-Based Bulk Metallic Glasses
Refraction Indices Measurement of Hexagonal Zeolite Crystal Using Brewster Angle Method
The Study of Electrochemical Property of Organic Coating on Magnesium Alloy
Notch Fatigue Properties of TRIP-Aided Annealed Martensitic Steels
Effects of Modification on Structure and Properties of Ramie Fiber/Polypropylene Composites
Comprehensive Analysis of High Nitrogen Steel Refining Factors with High-Pressure and Bottom-Blowing Nitrogen
Effect of Sr on the Microstructure and Properties of Hypereutectic Al-20 wt% Si Alloy
Research on Predicting the Stability of Partially Stabilized Zirconia Based on SVM
Sol-Gel Preparation of Fe-Doped TiO2 Loaded on HZSM-5 Zeolite
Flow Behavior of Heterocyclic Aramid Concentrated Solution
Reaction Synthesis and Oxidation Behaviours of Ludwigite
Effects of Ce Addition on the Mobility and Hot Tearing Tendency of Al-4.5Cu Alloy
Preparation and Property of SnXCuNiBi Solder Alloy
Recent Development in Multiscale Simulation of Mechanical Properties at Material Interface
Analysis Methods for the Tensile Behaviors of Woven Membrane Materials
Preparation of Ceramic Moulds with Zirconia Coatings for the Investment Casting of TiAl Alloys
Influences of Temperature on the Performance of Polypropylene Woven Geotextiles
Research on Predicting the Stability of Partially Stabilized Zirconia Prepared by Microwave Heating Using SVM
Influence of Melt Temperature on Compressive Plasticity of a Cu-Zr-Al Bulk Metallic Glass
Optimization of Piston Structure Aimed at Reducing Oil Consumption
Influences of Commercial SiC and Al2O3-SiC Synthesized from Clay on the Slag Resistance of Corundum Material
Research on Running Condition Recognition of Mechanical Equipment and Fault Diagnosis Method Based on Fuzzy Evaluation
Research on Rheological Behavior of Anion Gemini Surfactant Solution
Effects of Ramie Fiber Treatment on Thermo-Oxidative Properties of High-Density Polyethylene/Ramie Fiber Composites
Tearing Strength Calculation Model of the Synthetic Leather Base
Electrochemical Performance of LiFePO4 Coated by Nano-Polyaniline Coater for Lithium-Ion Batteries
Development of Piston Salt Core for the High Duty Engines
Non-Isothermal Crystallization Behavior in Zr55Cu30Ni5Al10 Bulk Metallic Glass
Design and Simulation of the Hydraulic System for the Rock Hob Test-Bed
Predicting Model in the Smelting Magnesium by Silicon-Thermo-Reduction Based on Artificial Neural Network
Percolation Phenomenon in Thermal Conductivity of Carbon Black Filled Rubber and Morphology
Effect of Multi-Wall Carbon Nanotube on Fracture Mechanical Property of Cement-Based Composite
Effect of Heat Treatment on the Corrosion Resistance of Cast Mg-7.3Al Alloy
Evaluation of Galactomannan from Gleditsia Sinensis Lam. as Sustained Release Material in Colonic Drug Delivery
Simulation of Shell Thickness Distribution and Flow Field in Slab Continuous Casting Mold
Experimental Study of Lattice Constant Dependence on the Grain Size in some Nanocrystallites
Asymptotic Crack-Tip Fields for Mixed Stationary Crack under Plane Stress Conditions in Pressure Sensitive and Elastic-Plastic Materials
Influence of Isothermal Annealing on the Micro-Hardness and Friction Property in CuZrAl Bulk Metallic Glass
Complexation of Cinnamon Essential Oil by ß-Cyclodextrin and its Release Characteristics at High Temperature
Dynamic Plastic Response of the Mg-Gd-Y Alloy over a Wide Range of Temperatures
Theoretical Study of Lattice Constant Dependence on the Grain Size in Some Nanocrystallites
Formation of Precipitations in Ultra-Low Carbon Microalloyed Steels Treated by Rapid Tempering
The Investigated Microstructure and Mechanical Properties of Al2O3/20wt% TiO2 Nanocomposite Coating
A Critique on Evaluating Fatigue Crack Propagation Properties Using Miniature Specimens
Slender Rack Processing Methods of Research and Practice
The Influence of HSO3- Activity on Electrochemical Characteristics of Copper
Research on Microstructure and Mechanical Property of the Production of Al-Si Alloy by Electric Warming
Study on Thermal Resistance of Basalt Filament Yarn
Research on the Surface Quality of ESR Large Slab Ingots
Evaluation of Mechanical Properties and Microstructures of Casing-Drilling Steels
Study on Microstructures and Mechanical Properties of Cold-Rolled C-Mn-Si-Al TRIP Steel
Investigation on Microstructure Evolution of Hot Deformed Free-Cutting Cu-Zn-Se-Bi-Sn Alloy
Underground Pumping Range Research and Practice
Influence of Si on the Electrochemical Performance of Al-Zn-In-Mg-Ti Sacrificial Anode Alloy
Large Deformation Analysis of Hyperelastic Membranes Containing a Hole or Inclusion
Study on Dynamic Recrystallization Behavior of Cu-Ni-Si Alloy
Microstructure and Crystallographic Texture of Oriented Silicon Steel Produced by TSCR
Study on Rolling Deformation Zone Feature of Corrugated Waist Rail
Characterization of Bisphenol a Poly(Carbonate) after Multiple Processing Cycles
Artificial Neural Network for Predicting the Flow Behaviors of Hot Compressed 2124-T851 Aluminum Alloy
Numerical Solution and Parameter Analysis of Structure with Different Modulus
Microstructure Evolution of Directionally Solidified Al-Cu Alloys
Microstructural Evolution and Mechanical Properties of AZ91 and SiCp/AZ91 Magnesium Alloys upon Rapid Solidification/Powder Metallurgy Followed by Hot Extrusion
Numerical Modeling of Granular Assembly Using Discrete Element Method
Microstructure and Texture Evolution during Recrystallization of Interstitial Free Steel
The Effect of Carbon on the Curie Temperature of Phase
Investigation of the Evaporation Processes of Gel Propellant Droplets
A Systematized FMEA Practice for Magnet Relays
Research on the CNC Machining Simulation Model Build and Realize Based on the Spiral Bevel Gear with Forming Method
Direct Deoxidation of ZrOCl2 Powder to Zirconium With Non-Sintering
Anelastic Behavior of Nanocrystalline Fe-Cr Alloy Obtained by Mechanical Alloying
Effect of Amino Acids on the Structure and Corrosion Resistance of Mg-Li Alloy Anodic Oxide Film
Damage Localization and Severity Estimate for Lattice Material
Research in Shape Meter Roll Deflection Compensation Model
Deformation Behavior and Dynamic Recrystallization of Hot Deformed GH625 Superalloy
Influence of Acid-Treated Carbon Nano-Tubes on the Microstructure and Properties of Carbon Nano-Tubes Polyurethane Composites
Acoustic Emission Study of Growth Process of Diamond Crystals under HPHT
Microstructure and Properties of Magnesium Alloy by Equal Channel Angular Processing
Effects of Solution Temperature on Microstructure and Tensile Properties of Casting Duplex Stainless Steel
Wear Behavior of AuAg/AgCuNiCe/Cu Commutator in DC Micromotor: A Case Study
Effect of Simulation Conditions on Grain Selection during Solidification of Single Crystal Casting
The Strucuture Transformation of Silicon Anode Material Induced by Lithium Ion Insertion
Nano-Scaled Fe3C Precipitates and Precipitation Strengthening in Hot Rolled Low Carbon High Strength Titanium Microalloyed Steel
Forming Limit of Holed Dome in Two-Stage Stretch Forming
Study on the Low-Temperature Resistance of Architectural Membrane Material by the Quadratic General Rotary Unitized Design
Thermogravimetry Analysis and Kinetic Characteristics of Ti(C,N) Formation by Slag-Coke Reaction
Laboratory and Field Test Study on Fly Ash as Subgrade Filling