This book was created from invited lectures and conference contributions of the "Metallography & Fractography 2022" conference, which is featured as an essential event for the presentation of results achieved in materials science and engineering. The conference participants come from universities, academic research institutions and different branches of industry with an interest in materials science and engineering. The conference also has strong support from companies that are experts in unique experimental equipment. The conference's ambition is regularly to expand the program to cover new approaches, new advanced materials and technologies, new findings in fundamental research and practical production, and to intensify international contacts.

Hornak / Matvija 18th Metallography and Fractography jetzt bestellen!

Weitere Infos & Material


Preface
Invited Lectures
Development of Materials for Solid State Hydrogen Storage
Slag from Modern Copper Production Found in Bergwerk, Burgenland, Austria
Influence of Surface Machining on Development of Stress Corrosion Cracking of Distribution Wheels of Main Circulation Pump in Nuclear Power Plants
Chapter 1: Microstructure, Properties and Processing of Structural Materials
Processing and Mechanical Properties of (Hf-Ta-Zr-Nb-Ti)C
Application of Composite Filament with the Addition of Metallic Powders in 3D Printing
Highly Accurate Structural Analysis of Austempered Ductile Iron Using EBSD Technique
Optimization of the Manufacturing Process of Sintered Fe-Mn-Cr-Mo-C Steels Using ANOVA
Direct Production of Tin Bronzes from Copper and Cassiterite
Microstructure-Properties Characterization of Selective Laser Melted Biomedical Co-28Cr-6Mo Alloy
Effect of Rare-Earth Doping on Dynamic Magnetic Properties of FeGa Alloy
Optimization of Raster Point Deposition Methodology for Deformation Analyses
Formation of Alpha-Case Layer during Oxidation of Ti6Al4V Surface by Annealing at 1050 °C and Change of Microstructure after Different Cooling Rates
Microstructure Analysis of Progressive Secondary AlSi7Mg0.6 Alloy with Higher Fe Content Using Electron Metallography Techniques
Comparison of Microstructure and Properties of Nickel-Copper Alloy Prepared by Casting and Laser Powder Bed Fusion Process
Formation of Sulphides in As-Cast GOES Thin Strips
Characterisation of a San Mai Steel Composite for the Manufacture of Knives
Numerical Simulation of the Welding Process during the Main Circulation Pump Impeller Repair
A Study of Cut Surface after the Abrasive Water Jet Application on the MS1 Material Prepared by DMLS Method
The Influence of Progressive Cladding Technologies on Layers Quality
Chapter 2: Corrosion
Identification of Corrosion Mechanisms of Stainless Steel with Metallography Cross Sections
Influence of Cavitation in Seawater on the Etching Attack of Manganese-Aluminum-Bronzes
Chapter 3: Fractographic Analysis
Microstructure and Fatigue Behavior of High-Performance Aluminum Alloy Al2024 Produced by Laser Powder Bed Fusion
Analysis of Cracks of Thermostats Casings Made of Brass
The Fractographic Analysis of Tensile and Fatigue Fracture Surfaces in Secondary A356 Aluminum Alloy with a Higher Concentration of Iron
Fracture Mechanisms of Austenitic Steel Caused by Dynamic Tests
High-Temperature Low Cycle Fatigue of Nickel-Based Superalloy IN738LC
Metallography of Fractured Aluminium Alloys for the Transmission System ´s Elements
Investigation of Fatigue Failure in Electric Locomotive Axle
Dynamic Fracture Characteristics of High-Strength Steel
Creep Resistance and Microstructure Evolution in HR3C-P92 Heterogeneous Welds
Analysis of Tribodegradation Factors Limiting the Life of the Molds
Chapter 4: Nanomaterials and Nanotechnologies
Preparation and Fracture Analysis of Advanced Layered Composite with Graphene-Coated Alumina Nanofibers
Influence of Ligands on Physicochemical Characteristics of Magnetic Nanoparticles
Carbon Fibers Doped by Binary Phosphides as an Electrocatalytic Layer for PEM Electrolysers
Chapter 5: Sample Preparation for Metallography
Evaluation of Sample Preparation Importance for Digital Image Correlation during Cold Deformation
Automation of Metallographic Sample Etching Process



Ihre Fragen, Wünsche oder Anmerkungen
Vorname*
Nachname*
Ihre E-Mail-Adresse*
Kundennr.
Ihre Nachricht*
Lediglich mit * gekennzeichnete Felder sind Pflichtfelder.
Wenn Sie die im Kontaktformular eingegebenen Daten durch Klick auf den nachfolgenden Button übersenden, erklären Sie sich damit einverstanden, dass wir Ihr Angaben für die Beantwortung Ihrer Anfrage verwenden. Selbstverständlich werden Ihre Daten vertraulich behandelt und nicht an Dritte weitergegeben. Sie können der Verwendung Ihrer Daten jederzeit widersprechen. Das Datenhandling bei Sack Fachmedien erklären wir Ihnen in unserer Datenschutzerklärung.